Description:
POLYONICS XF-434 is a Tedlar® (polyvinyl fluoride)
film with a permanent pressure sensitive acrylic adhesive and a high
opacity, yellow topcoat specifically designed for thermal transfer
or dot matrix printing.
Use: POLYONICS XF-434 is designed for barcode or
alphanumeric identification. When used with the proper ribbon, the
tag withstands many organic solvents, and especially fluids commonly
used in the aircraft and aerospace industries.
Properties: XF-434 has been tested for flame retardancy
per specifications of Boeing BMS 1347 J. Based on opur laboratory
tests it meets or surpasses these requirements.
| Properties |
Test
Methods |
Average
Results |
| |
|
USA
Units |
SI
Units |
| Thickness |
ASTM
D1000 |
|
|
| -Substrate |
|
0.0027
in. |
0.068
mm |
| -Adhesive |
|
0.0014
in. |
0.036
mm |
| -Total |
|
0.0041
in. |
0.104
mm |
| |
|
|
|
| Adhesion
to: |
ASTM
D-3330 |
|
|
| -Stainless
steel |
20
minute dwell |
>60
oz/in. |
|
| |
72
hour dwell |
82
oz/in. |
90
N/100mm |
| |
|
|
|
| Drop
Shear |
PSTC |
>100
hrs. |
>100
hrs. |
Temperature
range -40° F to 275°F (-40°C to 135°C)
All
Sl units are mathematically derived from U.S. conventional units.
Note. All values shown are averages and should
not be used for specification purposes. Test data and test results
contained in this document are for general information only and
shall not be relied upon by POLYONICS customers for designs and
specifications, or be relied on as meeting specified performance
criteria. Customers desiring to develop specifications or performance
criteria for specific product applications should contact POLYONICS
for further information.
WARRANTY-LIMITATION
Polyonics’ products are sold with the understanding that the
buyer will test them in actual use and determine for him/herself
their adaptability to his/her intended uses. Polyonics warrants
to the buyer that its products are free from defects in material
and workmanship, but limits its obligation under this warranty to
replacement of the products shown to Polyonics’ satisfaction
to have been defective, provided that the Purchaser has complied
with the handling, storage and shelf life requirements as specified
by Polyonics in applicable materials specifications. The Purchaser
shall return the products using Polyonics’ return policy as
stated above.
The above warranties extend solely to Purchaser and all warranty
claims must be made by Purchaser. Rework or Replacement shall neither
extend nor decrease the original warranty period. The term of all
warranty periods shall not exceed thirty (30) days from the date
of the original shipment.
THE ABOVE WARRANTIES ARE EXCLUSIVE OF AND IN LIEU OF ALL
OTHER WARRANTIES, WRITTEN OR ORAL, EXPRESS OR IMPLIED, STATUTORY
OF OTHERWISE. NO IMPLIED STATUTORY WARRANTY OF MERCHANTABILITY OR
OF FITNESS FOR A PARTICULAR PURPOSE SHALL APPLY. POLYONICS SHALL
NOT BE LIABLE EITHER IN TORT OR IN CONTRACT FOR ANY LOSS OR DAMAGE,
DIRECT, INCIDENTAL OR CONSEQUENTIAL, ARISING OUT OF THE USE OR INABILITY
TO USE THE PRODUCT, OR FROM DELAY IN THE REPLACEMENT OR REPAIR OF
PRODUCTS UNDER THE ABOVE WARRANTY.
Tedlar®
is DuPont’s tradename for its polyvinyl fluoride film.
|